Sharpening Taps and Hobs

Taps, like all other cutting tools, become dull through use. Dull taps can produce either oversize or undersize holes. They may chip, produce poor threads, or break in extreme cases.

Wear is greatly accelerated by the dullness of the tap. For example, a tap that has produced 2,000 tapped holes may be resharpened to its original usefulness with little effort and with the possibility of obtaining several additional sharpenings. However, if the same tap were allowed to produce 4,000 holes, it may be worn to a point where it is impossible to resharpen it satisfactorily. A determination of the number of holes to be produced by a tap must always include the factors of machine down-time for changing taps and the economic feasibility of resharpening. In many cases, it is most economical to run small taps until they will no longer produce satisfactory threads after which they are discarded. Larger and more expensive taps should be resharpened before wear becomes excessive.

Smaller sizes of taps are generally reconditioned by grinding the chamfer portion only, while larger taps may also require flute grinding. Taper pipe taps must be sharpened by grinding the flutes and spiral-pointed taps must be reground in the angular portion of the flute as well as on the chamfer.

In any type of reconditioning, it is generally advisable to duplicate the previous grind as close as possible. The chamfer must be true and uniform, and the original amount of relief should be maintained. Hand grinding of chamfers is not recomended; however if it is done, it should be done only in the simple fixtures or machines sold for this purpose.

Flute grinding or spiral point grinding should also be done on a tap reconditioning machine or on a cutter grinder. Flute grinding wheels should be shaped with a diamond dresser of appropriate type to produce a rake face or hook face as required. Both chamfers and flutes should be ground carefully so as not to burn the cutting edges of the tap, careful grinding will also produce a smooth finish on the tap. Wheels of K or L hardness and 60-grain or finer should be used.

    Tap Drill Size Calculator

    The size and condition of a hole before tapping has a direct bearing on the success of the tapping operation and the quality of thread produced. For best results, holes should be smooth and free of burrs. Drills should be kept sharp so that they cut freely. This is especially important in materials that work harden, such as some alloys and stainless steel. Reaming before tapping is desirable in all cases, and is a necessity for quality work, especially in the case of tapered threads.

    Often, the size of the hole before tapping is not clearly specified, or in many instances is specified without proper consideration of the factors involved. Misinformation on this matter can result in very high threading costs.

    American National and Unified thread specifications provide for a maximum of 83 1/3% thread. These specifications also provide a minimum value that varies from approximately 53% to 75%, depending upon the diameter and pitch of thread. In actual practice, however, the minimum percentage of thread required is generally determined by the design requirements of the thread involved. If the length of thread in the tapped hole is very short, it may be necessary to produce a minimum of 75% or 80% thread to develop the required strength. However, if the length of thread produced is several times the diameter, a 50% or 60% thread will usually provide a greater strength than that of the mating screw. Tapping costs increase very rapidly as the percentage of thread increases and it is poor economy to specify a greater percentage of thread than is actually necessary.To provide for practical tapping, the percentage of thread must be kept to a minimum in the cases of long thread lengths, fine pitches and small diameters.

    For example, it is entirely practical to produce a 1/4″-20 UNC thread of 80% in 1/8″ thick sheet metal; however, it would not be practical to produce this percentage of thread in a hole tapped to a 1/2-inch depth. Very fine pitch threads are difficult to tap with a high percentage even in the case of shallow holes.

    For the most economical tapping, the percentage of threads produced should always be as low as permissible, which means that the tap drill used should be the largest diameter that the specifications will permit. Minor diameters for various percentages of American National or Unified form of thread can be obtained by using the constants shown below – It must be remembered, however, that the values obtained are minor diameters and not drill sizes.

    Minor Diameter/Drill Size/ Percent of Thread – Chart »

    It is a well known fact that drills generally produce a larger diameter hole than the drill diameter, depending upon the condition of the drill, accuracy of the sharpening, etc., and also the material which is to be drilled.

    When tapping some materials, especially with fine pitch threads, a spin-up occurs at the crest of the thread so that the actual minor diameter of the thread after tapping is smaller than the size of the drilled hole. For this reason, the minor diameter of the tapped hole should be checked to make certain that it is within the limits specified. In other words, it may be necessary to experiment with various drill sizes to find the exact size that is satisfactory.

    Thread Rolling Considerations

    The Thread Rolling Paradox

    Theoretically, thread rolling is impossible because as a roll enters a blank, the ratio of diameters (roll to blank) is constantly changing. As a result, it would seem that the synchronization of the thread starts cannot be maintained. How then is thread rolling accomplished? The secret lies in the design of the thread roll holder, the selection of the roll diameter, and the design of the feed control cam on the machine tool.

    Straddle type thread roll holders, for example, have a certain amount of gear wind-up or hack-lash built in, that will accommodate corrective synchronization motion of the rolls during in-feed. There is also a small but critical amount of axial float provided for the rolls to further accommodate these self-adjusting motions. Next, the roll diameters are chosen so that the thread starts are in perfect synchronization when the rolls have achieved 50% penetration of the blank, thus minimizing the mismatch in diameters. Obviously, once full penetration of the blank has been achieved, it is important to remove the rolls from the blank as quickly as possible. Otherwise, the small amount of backlash provided by the holder will be consumed and the roll will start to strip the threads from the blank. That is where proper cam design comes in.

    How Threads Are Formed

    As the face of a thread die is forced against a rotating stock, the crest of the threads on the roll die begin to compress the work material. These initial points of contact will become the base or root of the rolled thread. As material is displaced by the penetration it is forced upward and outward from the side of the die thread flank, thus forming the crest of the roll thread on the blank. The nature of this
    flow of material must be taken into consideration.

    The 3 to 1 Ratio

    When a thread roll has almost reached its maximum penetration, the work on the outside diameter of the part will grow three times for every increment of additional penetration. In other words, if it is determined that a part is being made .003 inches under size, it will only require .001 inches additional die penetration to bring the diameter of the threaded part up to size. This is a very critical adjustment, for if a die penetration is too great, the root area of the roll die threads will be rapidly filled up, causing rapid wear or breakage of the thread roll. The most effective way to control the diameter on the finished part is through careful preparation of the blank.

    Thread Roll Troubleshooting

    Thread Filled Out In Center, But Not Towards Ends, Or Vice Versa


    1. Roll with varying diameter from end to end, or
    2. Blank with varying diameter from end to end.

    Split Thread – Axially


    1. Seamy stock, or
    2. Mark from shave tool or hollow mill

    Poor Finish On Thread


    1. Correspondingly poor finish on rolls, or
    2. Rolls that are worn out or broken, or
    3. Overfilling rolls, or
    4. Rolls not in match, or
    5. Material accumulated in threads on roll, or
    6. Material not ductile enough for cold-working

    Scuffed Crests


    1. Attachment not retracting fast enough, or
    2. Rolls and gear train binding, or
    3. Rolling beyond center line of work, or
    4. Material accumulated in threads on rolls

    Hollow Work, Hole Closes In


    1. Machine hole after rolling, or
    2. Needs supporting mandrel, or
    3. Feed rate too high, causing too rapid penetration

    Hollow Work, Hole Enlarged


    1. Machine hole after rolling, or
    2. Supporting mandrel too tight, or
    3. Blank too large on major diameter, or
    4. Feed rate too high causing too rapid penetration

    Hollow Work, Out Of Round


    1. Machine hole after rolling, or
    2. Feed rate too high causing too rapid penetration, or
    3. Too few work revolutions

    Have Questions?

    With facilities in Cheboygan, MI, and Cleveland, OH our extraordinary level of customer service translates into fast quote turnaround, outstanding technical support, reliable and available field support, and competitive lead times.

    Contact Us

    1306 Higgins Drive,
    Cheboygan, MI 49721

    800.633.3133

    NATLogo
    CCT Logo
    Name(Required)